Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 5.10 - 30.2 g/micron | 130 - 767 g/mil | Average value: 11.0 g/micron Grade Count:11 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Elmendorf Tear Strength, TD | 5.10 g/micron | 130 g/mil | |
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA) PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1.. |