Polymer Property : Elmendorf Tear Strength, TD = 465.6 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 18.33 g/micron
465.6 g/mil
ASTM D1922
SABIC 6821N Linear Low Density Polyethylene for Blown Film
Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi..