Polymer Property : Elmendorf Tear Strength, TD = 45.8 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 1.84 - 45.8 g/micron
46.7 - 1160 g/mil
Average value: 16.2 g/micron Grade Count:7
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..