Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 1.70 g/micron | 43.2 g/mil | ASTM D1922 |
Reliance Industries Relene E52009 Polyethylene Relene E52009 is a High Density Polyethylene grade with low gel content, excellent orientation characteristics and negligible water carry-over. This grade is recommended for making raffia tapes and.. |
|||
Elmendorf Tear Strength, TD | 1.70 g/micron | 43.2 g/mil | ASTM D1922 |
Eastman Tritan FX200 Copolyester Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Elmendorf Tear Strength, TD | 1.70 - 23.0 g/micron | 43.2 - 584 g/mil | Average value: 10.5 g/micron Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |