Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.80 g/micron | 122 g/mil | Calculated from mfr's report of 2.4 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® N196 Paper, 2 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Elmendorf Tear Strength, TD | 4.80 g/micron | 122 g/mil | ASTM-D1922 |
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all.. |
|||
Elmendorf Tear Strength, TD | 4.80 g/micron | 122 g/mil | ASTM-D1922 |
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the p.. |