Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.06 g/micron | 103 g/mil | 50 µm (2 mil) film; ASTM D1922 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |