Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 15.2 g/micron | 386 g/mil | ASTM 1922 |
Braskem Flexus® 9200 LLDPE Blown Film Extrusion Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing .. |
|||
Elmendorf Tear Strength, TD | 15.2 g/micron | 386 g/mil | ASTM-D1922 |
Braskem FM31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FM31D resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for blown film extrusion. It has excellent mechanical properties, especially hot tack. I.. |