Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 31.0 g/micron | 787 g/mil | ASTM D1922 |
Westlake Hifor Xtreme SC74860-F Polyethylene
(discontinued **) Hifor Xtreme Polyethylene SC74860-F is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more conventional 2.0-2.5 MI cas.. |