Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.30 g/micron | 83.8 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LA-0424-A LDPE Foam Resin Good stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film extr.. |
|||
Elmendorf Tear Strength, TD | 3.30 g/micron | 83.8 g/mil | |
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl.. |
|||
Elmendorf Tear Strength, TD | 3.30 g/micron | 83.8 g/mil | ASTM D1922 |
Braskem EB 853 LDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi.. |
|||
Elmendorf Tear Strength, TD | 3.30 g/micron | 83.8 g/mil | |
DuPont™ Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |