Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 11.7 g/micron | 298 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:.. |