Polymer Property : Elmendorf Tear Strength, TD = 28.5 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 22.8 - 28.5 g/micron
580 - 724 g/mil
ASTM D1922
BiologiQ ESR-PE EcoStarch mLLDPE Blend
Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin filmInformation provided by BiologiQ