Polymer Property : Elmendorf Tear Strength, TD = 28.3 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 28.3 g/micron
720 g/mil
ASTM D1922
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Stretch Wrap, CoextrusionsProcessing Conditio..
Elmendorf Tear Strength, TD 28.3 g/micron
720 g/mil
ASTM D1922
Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: processing aid additiveCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPEApplications: thick or t..
Elmendorf Tear Strength, TD 28.3 g/micron
720 g/mil
ASTM D1922
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene
For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
Elmendorf Tear Strength, TD 28.3 g/micron
720 g/mil
ASTM D1922
Dow DOWLEX™ 2083G Linear Low Density Polyethylene
Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
Elmendorf Tear Strength, TD 28.3 g/micron
720 g/mil
ASTM D1922
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A..