Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 18.7 - 26.0 g/micron | 475 - 660 g/mil | Average value: 22.6 g/micron Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |