Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 10.19 g/micron | 258.8 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug.. |
|||
Elmendorf Tear Strength, TD | 10.19 g/micron | 258.8 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C.. |