Elmendorf Tear Strength, TD 25.4 g/micron
645 g/mil
Dow DOWLEX™ 2267A Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2267A Polyethylene resin is a high performance blown film polymer offering superior load retention and toughness for a variety of stretch film packaging applications. This material complies..
Elmendorf Tear Strength, TD 25.4 g/micron
645 g/mil
ASTM 1922
Braskem LQ 0518/30 LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Heavy duty bags; shrink film. Information provided by Braskem