Polymer Property : Elmendorf Tear Strength, TD = 24.8 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 24.8 g/micron
630 g/mil
ASTM D1922
Chevron Phillips Dynex™ D605A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Elmendorf Tear Strength, TD 24.8 g/micron
630 g/mil
ASTM D1922
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE
Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi..
Elmendorf Tear Strength, TD 24.8 g/micron
630 g/mil
ASTM D1922
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE
Hexene Copolymer (High slip and antiblock)Applications: Blown film, general purpose filmBlown film, general purpose filmMeets all requirements of the U.S. Food and Drug Administration as specified i..
Elmendorf Tear Strength, TD 24.8 g/micron
630 g/mil
ASTM D1922
Formosa Plastics Formolene® L62009H Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administration as spec..
Elmendorf Tear Strength, TD 24.8 g/micron
630 g/mil
ASTM D1922
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles..
Elmendorf Tear Strength, TD 24.8 g/micron
630 g/mil
ASTM D1922
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of..
Elmendorf Tear Strength, TD 24.8 g/micron
630 g/mil
ASTM D1922
ExxonMobil LL 3201.22 Premium High Strength Film Resin  (discontinued **)
LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow..