Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 24.3 g/micron | 617 g/mil | ASTM D1922 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Elmendorf Tear Strength, TD | 24.3 g/micron | 616 g/mil | ASTM D1922 |
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Elmendorf Tear Strength, TD | 24.3 g/micron | 617 g/mil | |
Dow ATTANE™ 4403 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4403 copolymer is an ultra low density polyethylene having high impact, tear strength and exceptional flexibility. It is designed for use in industrial/consumer blown film applications and .. |