Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 9.06 g/micron | 230 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, TD | 9.06 g/micron | 230 g/mil | ASTM D1922 |
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom.. |