Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.09 g/micron | 53.0 g/mil | Calculated from mfr's report of 1.6 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |