Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.038 g/micron | 51.77 g/mil | ISO 6383-2 |
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco.. |