Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, TD = 17.2 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 5.12 - 17.2 g/micron
130 - 437 g/mil
Average value: 10.7 g/micron Grade Count:8
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a..
Copyright © lookpolymers.com All Rights Reserved