Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 6.08 g/micron
154 g/mil
ASTM D1922
Eastman Eastar A150 Copolyester, Film
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan..