Polymer Property : Elmendorf Tear Strength, TD = 14.8 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 14.8 g/micron
375 g/mil
ASTM D1922
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film
Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l...