Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 14.47 g/micron | 367.5 g/mil | ASTM-D1922 |
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional .. |