Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 14.1 g/micron | 358 g/mil | ASTM D1922 |
Huntsman Rexell® H3108 Cast Film Extrusion LLDPE
(discontinued **) Linear low density octene copolymerApplications: Cast film extrusionFilm properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by Huntsman Corporation |