Polymer Property : Elmendorf Tear Strength, TD = 13.12 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 13.12 g/micron
333.2 g/mil
ASTM-D1922
Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer
LF 118/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prop..