Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 12.8 g/micron | 325 g/mil | ASTM D1922 |
ExxonMobil Pax-Plus™ 3204 Blown Film Resin Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin.. |