Polymer Property : Elmendorf Tear Strength, TD = 117 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 4.60 g/micron
117 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film
The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc..
Elmendorf Tear Strength, TD 4.60 g/micron
117 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film
The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product..
Elmendorf Tear Strength, TD 4.60 g/micron
117 g/mil
ISO 6383-2
Total XSene® HD55110 High Density Polyethylene - Blown Film
HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl..