Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 0.275 g/micron | 6.99 g/mil | ISO 6383/2 |
Borealis Borstar® FB2230 LLDPE for Film Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Elmendorf Tear Strength, TD | 0.275 - 135 g/micron | 6.99 - 3430 g/mil | Average value: 21.8 g/micron Grade Count:175 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |