Polymer Property : Elmendorf Tear Strength, MD = 79.5 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 3.13 g/micron
79.5 g/mil
ASTM-D1922
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene
TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes..