Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 70.0 g/micron @Thickness 0.0150 mm |
1780 g/mil @Thickness 0.000591 in |
ASTM D1922 |