Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 1.65 g/micron | 42.0 g/mil | ASTM D1922 |
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE