Elmendorf Tear Strength, MD 3.8722 g/micron
98.354 g/mil
ISO 6383-2
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene
Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire..