Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 3.33 g/micron | 84.6 g/mil | ASTM-D1922 |
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the p.. |