Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 2.2418 g/micron | 56.942 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |