Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD >= 7.48 g/micron
>= 190 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 5118Q (18603) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD 7.48 g/micron
190 g/mil
ASTM D1922
Chevron Phillips MarFlex® 5430 Low Density Polyethylene, Cast Film
This LDPE is tailored for cast film applications that require:Excellent opticsEasy processingHigh coefficient of frictionTypical cast film applications include:OverwrapCoextruded filmGeneral purpose..
Elmendorf Tear Strength, MD 7.48 g/micron
190 g/mil
ASTM D1922
Chevron Phillips MarFlex® 5440 Low Density Polyethylene, Cast Film
This LDPE is tailored for cast film applications that require:Suited for high speed convertingGood clarityLow coefficient of frictionTypical cast film applications include:Coextruded filmGeneral pur..