Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 7.20 g/micron | 183 g/mil | ASTM-D1922 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |