Polymer Property : Elmendorf Tear Strength, MD = 155 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 6.10 g/micron
155 g/mil
ASTM D1922
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin
Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid..
Elmendorf Tear Strength, MD 6.10 g/micron
155 g/mil
ASTM D1922
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin
Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide..
Elmendorf Tear Strength, MD 6.10 g/micron
155 g/mil
ASTM D1922
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film
Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l...
Elmendorf Tear Strength, MD 6.10 g/micron
155 g/mil
ISO 6383-2
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film
Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion ..