Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 5.71 - 5.91 g/micron | 145 - 150 g/mil | (direction not reported), Propagation Tear Strength; ASTM D-1922 |
Saint-Gobain Norton® FEP Fluoropolymer Film Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp.. |