Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 13.247 g/micron | 336.47 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by .. |
|||
Elmendorf Tear Strength, MD | 13.247 g/micron | 336.47 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e.. |
|||
Elmendorf Tear Strength, MD | 13.247 g/micron | 336.47 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |