Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 5.08 g/micron
129 g/mil
50 µm (2 mil) film; ASTM D1922
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res..
Elmendorf Tear Strength, MD 5.09 g/micron
129 g/mil
ISO 6383/2
Borealis Borstar® FB2310 LLDPE for Film
Borstar BF2310 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from ..