Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | >= 47.2 g/micron | >= 1200 g/mil | (direction not reported), Propagation Tear Strength; ASTM D-1922 |
Saint-Gobain Norton® ECTFE Fluoropolymer Film Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon.. |