Polymer Property : Elmendorf Tear Strength, MD = 12.3 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 12.3 g/micron
312 g/mil
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade
DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev..