Polymer Property : Elmendorf Tear Strength, MD = 11.2 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 11.2 g/micron
284 g/mil
ASTM D1922
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin..