Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 4.06 g/micron | 103 g/mil | 50 µm (2 mil) film; ASTM D1922 |
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |