Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 1.80 g/micron | 45.7 g/mil | ASTM D1922-67 |
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used.. |
|||
Elmendorf Tear Strength, MD | 1.80 g/micron | 45.7 g/mil | ISO 6383-2 |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Elmendorf Tear Strength, MD | 1.80 g/micron | 45.7 g/mil | ISO 6383-2 |
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch .. |
|||
Elmendorf Tear Strength, MD | 1.80 g/micron | 45.7 g/mil | ISO 6383-2 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |