Polymer Property : Elmendorf Tear Strength, MD = 1.54 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.54 g/micron
39.0 g/mil
Calculated from mfr's report of 1.2 N per TAPPI-414 and the typical thickness
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..