Elmendorf Tear Strength, MD 0.250 - 70.0 g/micron
6.35 - 1780 g/mil
Average value: 1.82 g/micron Grade Count:67
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Elmendorf Tear Strength, MD 0.250 g/micron
6.35 g/mil
ASTM D1922
SCG Chemicals EL-Leneâ„¢ F15 High Density Polyethylene Film
Key Characteristics:High productivityHigh tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierExcellent printabilityRecommended Applications:High speed processingWide l..
Elmendorf Tear Strength, MD 0.250 g/micron
6.35 g/mil
ASTM D1922
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film
Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor..
Elmendorf Tear Strength, MD 0.250 g/micron
6.35 g/mil
ASTM D1922
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film
Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film (