Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 0.0217 - 1.87 g/micron | 0.550 - 47.5 g/mil | Average value: 0.575 g/micron Grade Count:5 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Elmendorf Tear Strength, MD | 0.0217 g/micron | 0.550 g/mil | ASTM D1922 |
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: This SBC is easily processed on blown film or cast fi.. |
|||
Elmendorf Tear Strength, MD | 0.0217 g/micron | 0.550 g/mil | ASTM D1922 |
Chevron Phillips K-Resin® DK11 Styrene-Butadiene Copolymer, Film Grade Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: Provides the same high performance film properties as.. |