Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 6.27 MPa
910 psi
at 2% offset; ASTM D882
ExxonMobil Escorene® LD 319.92 Film Resin  (discontinued **)
Escorene Ultra LD 319.92 is a 9.0 wt% vinyl acetate copolymer film resin, that exhibits superior impact strength and heat sealability.Information provided by ExxonMobil Chemical